(Summary description)1. If the die casting products appear black and flow marks, the pouring temperature and mold temperature should be appropriately increased;

2. If the alloy composition does not meet the standard, the alloy composition should be changed to improve fluidity;

3. See the flow direction of the molten aluminum when the mold is hot. The cold partition caused by the collision of the molten metal appears vortex-like with flow marks. The gating system should be improved to improve the filling direction of the inner gate. In addition, a slag bag can be set up at the edge of the casting to improve the filling conditions;

4. If the distal end is not compacted, the gate position and cross-sectional area should be changed to improve the overflow conditions and increase the overflow flow;

5. The product is dark and often accompanied by surface bubbles, so the injection speed must be increased correctly;

6. The overall pressure of the casting is not compact, and the injection pressure is relatively low, so the specific pressure should be increased appropriately.

Cold isolation and cold joint (butt joint) of die casting surface defects

(Summary description)1. If the die casting products appear black and flow marks, the pouring temperature and mold temperature should be appropriately increased;

2. If the alloy composition does not meet the standard, the alloy composition should be changed to improve fluidity;

3. See the flow direction of the molten aluminum when the mold is hot. The cold partition caused by the collision of the molten metal appears vortex-like with flow marks. The gating system should be improved to improve the filling direction of the inner gate. In addition, a slag bag can be set up at the edge of the casting to improve the filling conditions;

4. If the distal end is not compacted, the gate position and cross-sectional area should be changed to improve the overflow conditions and increase the overflow flow;

5. The product is dark and often accompanied by surface bubbles, so the injection speed must be increased correctly;

6. The overall pressure of the casting is not compact, and the injection pressure is relatively low, so the specific pressure should be increased appropriately.

  • Categories:company news
  • Author:
  • Origin:
  • Time of issue:2021-01-08
  • Views:0
1. If the die casting products appear black and flow marks, the pouring temperature and mold temperature should be appropriately increased;
 
2. If the alloy composition does not meet the standard, the alloy composition should be changed to improve fluidity;
 
3. See the flow direction of the molten aluminum when the mold is hot. The cold partition caused by the collision of the molten metal appears vortex-like with flow marks. The gating system should be improved to improve the filling direction of the inner gate. In addition, a slag bag can be set up at the edge of the casting to improve the filling conditions;
 
4. If the distal end is not compacted, the gate position and cross-sectional area should be changed to improve the overflow conditions and increase the overflow flow;
 
5. The product is dark and often accompanied by surface bubbles, so the injection speed must be increased correctly;
 
6. The overall pressure of the casting is not compact, and the injection pressure is relatively low, so the specific pressure should be increased appropriately.
Search
Search
Cancel
 Yangzhou Qiyuan Automobile Mould Manufacturing Co., Ltd

General manager Guo:13852210520

Mobile:13852208885

A professional manufacturer of various cab mold manufacturers. The company uses UG, CAM technology for the design and processing of complete sets of mold.

 Yangzhou Qiyuan Automobile Mould Manufacturing Co., Ltd